Just a quick post to illustrate the quality of finish I use, which is Flex Coat epoxy resin, and the variety of rod types that can be dealt with.
Dave from Stockport phoned after a search on the net in a bit of a panic on a sunday as he had a sea trip planned the following friday, amd two boat rods both with broken butt rings !
As I'm always happy to try and accommodate where possible, and as I had a day or two to wait for reel parts I was able to slot him in in-between jobs. The rings weren't an exact match in shape, the rings on the rod were the older, flimsier version of the one below, which are notorious for not being able to take a knock or bang !
(no offense to the ring pictured which is actually a decent type!)
So when the rods were dropped off I actually made a start on them the same day, applied the finish over the next couple of days as it was quite a thick finish, and the end result is pictured below, not too shabby at all ;)
I didn't get an exact match on the red coloured whipping but not a million miles away either and Dave was made up to be getting out so another happy customer!
Repairs, reel servicing & rod building from (ex) Trafford Angling Supplies longest serving staff member Dave,
with over 25 years in the industry, and creator of the TBR2 Barbel Tripod.
with over 25 years in the industry, and creator of the TBR2 Barbel Tripod.
Showing posts with label rod repair. Show all posts
Showing posts with label rod repair. Show all posts
Thursday, 24 September 2015
Friday, 18 September 2015
Free Spirit Launcher Spod Rod butt ring repair pre-finish shots
Just a couple of quick pic's of a butt ring repair to a Free Spirit spod rod, quite possibly my 'favourite' brand to repair !
The blanks really are great to work on and always come out really well, the factory finish is pretty much bullet proof and very difficult to mark, very much a case of - you get what you pay for - and it shows.
If you ever wanted a set of rods as 'an investment' you'd be hard pushed to better them, no offense to Century or Harrison ;)
Anyway, the finish to match is what I'd call 'extra-thick', so I prefer to do it in 2 stages, first stage shown here. This coats and sinks into the whipping thread, securing it to to the blank, I'll leave this 24 hours before applying the top finishing coat, it can be done in one, but this gives me the chance to tweak and adjust it so it comes out as perfect as a factory finish, I don't get any complaints.
;)
The blanks really are great to work on and always come out really well, the factory finish is pretty much bullet proof and very difficult to mark, very much a case of - you get what you pay for - and it shows.
If you ever wanted a set of rods as 'an investment' you'd be hard pushed to better them, no offense to Century or Harrison ;)
Anyway, the finish to match is what I'd call 'extra-thick', so I prefer to do it in 2 stages, first stage shown here. This coats and sinks into the whipping thread, securing it to to the blank, I'll leave this 24 hours before applying the top finishing coat, it can be done in one, but this gives me the chance to tweak and adjust it so it comes out as perfect as a factory finish, I don't get any complaints.
;)
Sunday, 23 August 2015
Century Spod Rod butt ring repair part 1. . . . . . . . . . . . .
Century Spod Rod butt ring repair part 1. . . . . . . . . . . . .
Part 1 ??
Yes, I have aways preferred to do finishes as thick as Century paste them on in 2 stages, first coat semi-thick to set the whippings in place, which can then be adjusted and tinkered with if need be, then the second coat is applied 24 hours later, to achieve a perfect 'factory finish' that most can't tell apart from the original.
This is stage one in the images below, brand new 40mm Kigan ring on a Century Big Bertha Spod rod . . . . . . . . . . . . .
Watch this space for part 2 !
Part 1 ??
Yes, I have aways preferred to do finishes as thick as Century paste them on in 2 stages, first coat semi-thick to set the whippings in place, which can then be adjusted and tinkered with if need be, then the second coat is applied 24 hours later, to achieve a perfect 'factory finish' that most can't tell apart from the original.
This is stage one in the images below, brand new 40mm Kigan ring on a Century Big Bertha Spod rod . . . . . . . . . . . . .
Watch this space for part 2 !